Specifications
PN# | TDF-15/250-PM | TDF-25/400-PM | ||
Optical specifications | Operating wavelength | nm | 1900-2100 | 1600-2100 |
Fiber Core NA | - | 0.11±0.02 | 0.10±0.01 | |
Fiber cladding NA | - | ≥0.46 | ≥0.46 | |
Cladding attenuation @860nm | dB/km | ≤15.0 | ≤15.0 | |
Cladding absorption @793nm | dB/m | 2.2±0.2 | 2.2±0.2 | |
Birefringence coefficient | 10-4 | 3.0±0.5 | 3.0±0.5 | |
Dimensions & Mechanical specifications | Fiber core diameter | μm | 15.0±1.0 | 25.0±2.0 |
Cladding diameter | μm | 250.0±5.0 | 400.0±5.0 | |
Cladding shape | - | Circle,Panda | Circle,Panda | |
Coating diameter | μm | 395±10.0 | 550±15.0 | |
Coating materials | - | Low refractive index coating | Low refractive index coating | |
Matrix material | - | Quartz | Quartz | |
Screening strength | kpsi | ≥100 | ≥100 |